Moulding Process & Quality
A PA66 Part Gains 2.7% Water at Room Humidity and Loses 61% of Its Stiffness (Data From Two Resin Makers)

PA66 leaves the press dry, then takes on 2.7% moisture at room humidity and 8.5% soaked. Datasheet figures show what that water does to size and stiffness.
Two of Five Moulding Resins Break Down Without a Dryer (6 Processing Guides Checked)

PC needs 120 °C for 2–3 h at 0.02% moisture; PA66 needs 4 h at 80 °C; ABS 2–4 h; PP and PE usually skip the dryer. Six manufacturer processing guides compared.
Flat Parts Do Not Warp From One Bad Setting: 3 Peer-Reviewed Studies Rank Packing Pressure First and Gate Size Last (0.3% vs 1.1% Datasheet Pair)

Three published studies rank packing pressure first for thin-wall warpage and gate size last. One datasheet pair shows a 0.3 vs 1.1 percent shrinkage split.
A Small Shot on a Big Barrel Degrades Before the Mould Opens: Keep the Metering Stroke at 1–3 D (5 Resin Limits, 2 Supplier Rules)

A 45 g shot on a 900 g barrel waits 10.7 min per 32 s cycle. Durethan PA grades cap at 4–10 min in the cylinder. Check barrel occupancy beside clamp tonnage.
Resin Up 2,900 Yuan/t and Tariffs Stacked to 37.5%: When Mold Flow Analysis Earns Its Line Item in a Mould RFQ

Resin prices and stacked tariffs make scrap costlier in 2026. See when mold flow analysis earns its line item in a mould RFQ, and when a DFM review covers it.
Raising Injection Pressure Will Not Save a Glass-Filled Weld Line: Measured Retention Data for Your RFQ (2 Peer-Reviewed Studies)

Peer-reviewed tests put PP-GF20 at 28.1 MPa across a weld line against 52.3 MPa without one. See which process levers move that number before you send your RFQ.
Ribs at 60 Percent of Wall Can Still Sink a Gloss Panel: Check the Root Circle, Not Just the Ratio (3 Sources, 1 Measured Test)

Design guides allow ribs at 50 to 60 percent of wall, yet gloss panels still sink. A measured PC study found 0.25 to 0.34. The rib root circle explains the gap.
A 6 mm Runner Adds 26% Resin to a 12 g Part: Size the Channel Before the Steel Is Cut (4 Resins, 20 Sizes)

A 6 mm cold runner holds 3.07 g of PP per 120 mm, or 25.6% extra resin on a 12 g part. Channel weights for four resins, plus the sizing checks to run first.
12.7 mm of Retainer-Plate Float Cuts an Ejector Pin’s Buckling Load by 36% (12 Pin Sizes Calculated)

Ejector pins rarely break from bad steel. Keep the unsupported span under 25 times the pin diameter, and each pin still carries 3x a 276 MPa cavity load.
Cavity Count Cuts the Part Price, Then Melt Balance Takes Part of It Back (8-Cavity Mould, 26.15 mm Measured Spread)

More cavities cut machine time per part, but published trials show a balanced 8-cavity mould still fills as two melt streams, with fill spread up to 26.15 mm.