Moulding Process & Quality
A 2–4 µm Film Beats Bulk Hardness Against Glass-Filled Resin (90,000-Shot Mould Test)

PVD films 2–4 µm thick multiply mould life on glass-filled resin. A 90,000-shot trial ranks coatings differently from lab tests. Here is what holds up.
A sink EDM leaves a 3.7-53 µm white layer on H13, and no CMM report will show it (3 studies)

An EDM white layer runs 3.7 to 53 µm deep on die steel, harder than the metal beneath it. A CMM cannot see it. Stone past the layer before the mould ships.
Eight grit steps from an as-EDM cavity to SPI A-1, four to B-2: what a finish callout really buys (12 grades mapped)

Twelve SPI grades sit four to eight grit steps apart from the same EDM surface. Per-face grades and a finer EDM finish cut polishing hours and the tooling bill.
Boss Walls Range From 0.50T to 0.75T in Three Design Guides. Interference, Not Wall, Decides Which One Cracks

Three design guides put the screw-boss wall between 0.50 and 0.75 of nominal wall. Bore stress explains why: interference, not wall thickness, cracks the boss.
Doubling Injection Speed Doubled Flash Area: Rank the Gaps, Speed and Hold Pressure Before You Add Clamp Tonnage (16-Run DOE)

Flash follows gaps and pressure, not clamp shortfall. A 16-run DOE ranks speed first; a 400 t on 100 t case crushed vents. Shut-off fixes from the toolroom.
PC snap arms survive 4% strain before they crack: 5 housing resins ranked by deflection limit

PC snap arms hold 4% strain before they crack. PC/ABS allows 2.5% and 20% glass-filled PC only 2.0%. Friction cuts it, so grade and mould decide the lid.
Melt Flow Rate Decides the Gate Before the Steel Is Cut: Read the Condition, Not Just the Number (5 Datasheets, ISO 1133)

Melt flow rate shapes gate size, wall limits and press choice. Five official datasheets show why the condition column decides if the number means anything.
Notched Impact Fell from 530 to 100 J/m in Three Passes – Your Regrind Cap Decides Which End You Land On (3 Trials)

A closed runner loop puts 1.43 heat histories on every pellet, and notched impact falls from 530 to 100 J/m. Size the regrind cap together with the runner.
Part Weight Levels Off When the Gate Seals: Size the Holding Phase by the Plateau (600 bar Test)

Holding pressure past gate seal adds cycle seconds and runner waste, never part weight. A 16-cavity ABS test froze its gates in about two seconds at 600 bar.
A 5% Undercut Is the Strip Line, Until Glass Fibre Cuts It to 1% (3 Resin Families)

Undercuts strip to 5% of diameter in acetal, 6 to 10% in unfilled nylon, 1 to 2% in glass-filled nylon. The lifter trigonometry sets the rest of the tool cost.