Most drawings we receive name a finish in one of two ways. Some carry a grade, usually SPI B-2 or A-2. Others carry a word, and the word is almost never measured: high gloss, smooth, matte, like the sample.

Two quoting habits sit behind that gap. One shop prices finish as a single line and applies it to the whole cavity. Another shop prices it face by face, and the two numbers for the same part can differ by more than the steel does.

The disagreement is not about taste. The same twelve-grade chart gets read as a linear scale from dull to bright, when the real cost driver is the number of abrasive steps and the area each step covers. Published Ra bands also stop agreeing once the chart reaches the blasted grades.

Four questions guided this breakdown:

  • What Ra band does each of the twelve SPI grades actually carry?
  • How many grit steps separate an as-EDM surface from A-1 and from B-2?
  • Why does the EDM recast layer consume the first steps regardless of the target grade?
  • Which faces on a drawing deserve a polished grade at all?

The short version: count steps and measure area, then pick the grade. The grade name tells a buyer almost nothing about the hours inside the quote.

Here is the case in one paragraph. From a cavity left at roughly Ra 1.6 µm by a semi-finish EDM pass, reaching SPI B-2 at 0.15 µm takes about four abrasive steps, and reaching A-1 at 0.012 µm takes about eight. Dropping the EDM finish to 0.4 µm before benching removes two of those steps at either grade. The recast layer left by a roughening pass, commonly 15 to 30 µm thick, is deeper than the first two stone stages can cut, so a grade A target on an unfinished EDM surface sends diamond compound into damaged steel. Polishing hours scale with steps times area, and that product, not the grade word, is what a tooling quote is pricing.

Key takeaways

  • Grade spread: the twelve SPI grades run from Ra 0.012 µm at A-1 to a band that published charts put between 3.2 and 18 µm at D-3.
  • Step count: from an Ra 1.6 µm EDM surface, B-2 needs 4 abrasive steps, A-3 needs 5, and A-1 needs 8.
  • EDM finish pays twice: a 0.4 µm EDM finish instead of 1.6 µm cuts 2 steps off every grade from B-2 upward.
  • Recast first: a roughening pass leaves 15 to 30 µm of recast, deeper than two stone stages remove, so it must be cut back before diamond work starts.
  • Area, not grade: a 200 cm² cavity taken to B-1 carries more polishing time than a 20 cm² visible face at A-2, because hours follow steps times area.
  • Defaults that work: B-2 on hidden walls, A-3 on gloss faces, and 2 written grades on the faces a user touches.

Methodology

The grade list comes from the SPI classification now maintained by the Plastics Industry Association as the AR-106 Mold Finish Guide, a plaque set plus a 43-page document published in 2014. The standard is sold as a physical reference, and the Ra bands below come from published reproductions of that chart rather than from the document itself.

Bench practice comes from MoldMaking Technology interviews with a polishing trainer, and from a shop case on electrochemical polishing. Both describe what happens to a surface between EDM and final buff, and neither is a controlled trial.

The step counts are arithmetic done in our tooling office, not measurements. We assume each abrasive stage roughly halves Ra, then round up to whole steps. Nobody in our plant runs a roughness tester on cavity steel, so treat the counts as a planning model and not as inspection data. Shop input here is limited to process routing: copper electrodes cut on site, EDM and surface grinding in the same building, and cavity plates measured on the bridge CMM before trials.

What Ra does each SPI grade carry, and where do the numbers come from?

Twelve grades, four families, and one warning. The families are buffed, paper, stone and blasted, and each family moves in steps of its own.

SPI gradeAbrasive stageTypical Ra band (µm)
A-1Grade #3 diamond buff0.012 – 0.025
A-2Grade #6 diamond buff0.025 – 0.05
A-3Grade #15 diamond buff0.05 – 0.10
B-1600 grit paper0.05 – 0.10
B-2400 grit paper0.10 – 0.15
B-3320 grit paper0.28 – 0.32
C-1600 grit stone0.35 – 0.40
C-2400 grit stone0.45 – 0.55
C-3320 grit stone0.63 – 0.70
D-1Glass bead blast0.80 – 1.00
D-2#240 aluminium oxide1.00 – 2.80
D-3#24 aluminium oxide3.20 – 18.0

Read A-1 through C-3 first. Charts that reproduce the SPI table agree on those bands to two decimals. Read D-1 through D-3 with suspicion, because published versions of the same chart disagree there, and one version puts D-3 at 4.0 to 8.0 µm instead of 3.2 to 18.0.

The bands are not tolerances. A grade describes an abrasive route and an appearance, and Ra is the measurable side effect of that route.

A second, older ladder is worth knowing. Mirror polishing in Asian toolrooms is often spoken in A0 to A4 terms, where A0 is Ra 0.008 µm and A4 is 0.063 µm. Those labels sit beside the SPI scale rather than inside it.

How many grit steps sit between an EDM surface and each grade?

One assumption drives this table: each abrasive stage removes the previous scratch pattern and lands at roughly half the roughness. Step counts then follow from the ratio between the starting surface and the target band.

Target gradeTarget Ra (µm)From Ra 1.6 µmFrom Ra 0.8 µmFrom Ra 0.4 µm
B-20.154 steps3 steps2 steps
B-10.0755 steps4 steps3 steps
A-30.055 steps4 steps3 steps
A-20.0256 steps5 steps4 steps
A-10.0128 steps7 steps6 steps

Eight steps against four sounds like double the work. It is worse than that in practice, because finer abrasives cut less per pass at the same pressure.

The column that matters for a quote is the gap between columns. Going from a 1.6 µm EDM finish to a 0.4 µm one costs machine time once and saves steps on every grade the part needs.

Multi-cavity mould plate with cooling ports and inserts checked on the assembly bench

A multi-cavity plate on the bench, checked before trials. Every cavity face in this stack carries the same grade on most drawings, and that is the expensive default.

Why does the recast layer eat the first steps, whatever the target grade?

EDM leaves more than a roughness value. Each spark melts a small pool of steel that quenches against cold metal, and the result is a hard, brittle layer on top of sound material. That layer has to go before any polished finish can be trusted.

EDM stageTypical recast depthWhat the bench has to do
Roughening pass only15 – 30 µmCut back damaged steel before any fine abrasive
Semi-finish pass5 – 15 µmStone through the layer, then start the paper sequence
Fine skim pass1 – 5 µmOne stone stage, then straight to paper
Electrochemical polish after EDMLayer removed, about 0.1 mm of surface dissolvedStart fine work on clean steel

Recast depth is quoted across the industry, not measured by us. The useful comparison is scale. A 15 µm layer of damaged steel is thicker than two stone stages remove. Those two stages restore steel instead of chasing gloss.

A polishing trainer quoted in MoldMaking Technology makes the same point from the other end. Pads that arrive shiny from high-speed milling tempt a polisher to start at 600 or 900 grit, and that fails because the hard layer under the shine is still there. He starts at 400 grit instead, and warns that hard particles from EDM can break out mid-polish and leave a pit.

Electrochemical polishing offers a shortcut that fits complex geometry. The shop case reports roughness after EDM cut by up to seven times, at 40 to 80 A/cm² across a 0.1 to 0.5 mm gap, with the layer dissolved rather than abraded. Fine diamond work still follows, but it starts on sound metal.

Which faces should carry a polished grade?

Split the drawing by what a user sees and touches. A whole cavity at one grade is the most common overspend we see in incoming drawings, and it is also the easiest to fix.

Face on the partGrade that usually holdsReason
Visible gloss face on a housingA-3Reflects light, hides less than a mirror, prices well below A-2
Clear or light-guide partA-2 to A-1Haze and flow marks show through the part, so both halves get polished
Hidden structural wallB-2 or C-1Release and tool marks are the only concerns
Grip or decorative patternD-1 to D-2, or a texture gradePattern hides marks and reduces polishing to zero on that face
Shut-off land and sealing faceGround, not polishedFlatness and contact decide flash, and grinding holds both

Take the clear-part row seriously. A polished cavity opposite a stoned core gives a part that reads cloudy from one direction. Buyers spot that before they spot gloss.

Multi-cavity moulded automotive parts laid out on a bench after a trial run

Parts from a trial run, laid out for comparison. Finish differences across cavities show up here long before a gloss reading does.

Materials shift the outcome as much as the grade does. Polycarbonate and acrylic hold a high polish. Polypropylene and polyethylene shrink more and show sink and flow marks, and a mirror cavity makes those marks louder.

Limitations

The step counts are a model, and a model can be wrong in both directions. A soft steel that tears under a stone needs more stages than the ratio predicts, and a well-controlled skim pass can need fewer.

Bench behaviour and moulding behaviour are separate questions. A cavity that reads uniform under bench light can still show a flow line on the part, because filling, packing and cooling decide the surface as much as the steel does. Nothing in this table tells a buyer what a trial shot will look like.

The third-party numbers carry their own limits. Recast depth ranges come from published EDM practice and vary with current, pulse time and flushing. The Ra bands are reproductions of a standard sold as a plaque, and the reproductions disagree at the blasted end. None of these sources inspected the tool in front of you.

What this means for your RFQ

We help product teams spend their finishing budget on the faces that get looked at. That starts with a drawing that names a grade per face instead of one grade for the whole tool.

Three lines on the drawing do most of the work. Mark the cosmetic faces and give each one a grade. State the EDM finish you expect on unpolished faces, so the bench inherits a known starting point. Say whether the part is clear, because clear parts double the polished area.

Send a 2D drawing with those callouts, or a 3D file plus a marked photo of the visible surfaces, to info@hongqiangmould.com. A tooling price with the finish split by face comes back inside 24 hours, and the split is where most of the savings sit. Copper electrodes, EDM, surface grinding and the CMM run under one roof here, so a grade change is a routing decision rather than a subcontract.

One line worth keeping on any drawing: polish where it shows, stone where it does not.

Mapped | Stepped | Quoted

Frequently asked questions

Is SPI A-1 twice as expensive as SPI B-2? Not on a fixed multiplier. The step count goes from about four to about eight, and each finer step cuts less material per pass. Area multiplies the difference, because polishing hours follow steps times polished surface. A small optical insert at A-1 can price below a large housing cavity taken to A-2 over every wall.

Can an EDM finish skip straight to diamond compound? No. Rough and semi-finish EDM passes leave a hard recast layer between 5 and 30 µm deep, and diamond work polishes that layer rather than the steel under it. Pits then appear as the hard particles break away. One or two fine skim passes, or an electrochemical step, cut the layer back first.

Which grade should a drawing use when the buyer has no preference? B-2 covers most opaque parts, because it removes tool marks and releases cleanly without diamond time. Add A-3 only on faces a user looks at under light. Adding A-1 to a part that is not clear or optical buys polishing hours nobody will see.

Does a polished cavity improve part strength or only appearance? Appearance is the main effect, with one exception. A smoother cavity reduces drag during ejection, which helps on deep walls and soft resins. Strength comes from wall design, gate position and packing. Do not expect a finer grade to rescue a part that warps or sinks.

Jack works on the tooling and molding team at Hongqiang Mould, a mould shop in China that builds injection moulds and runs production moulding on 11 presses from 80 to 450 T. He writes about the numbers behind tooling decisions: clamp force, cooling, ejection and the tolerance stack that decides whether a part assembles.

Sources

Mold Finish Guide, AR-106. Plastics Industry Association, ANSI/SPI, 15 Jan. 2014, access.plasticsindustry.org/plasticsindustry/PLASTICS/CustomPages/PLASTICS_Store_Home.aspx.

How to Polish an Injection Mold? Injection Moulding Reference, injectionmould.org/?p=2258.

Rethinking How to Polish. MoldMaking Technology, moldmakingtechnology.com/articles/rethinking-how-to-polish.

International Perspective: The Electrochemical Mold Polishing Advantage. MoldMaking Technology, moldmakingtechnology.com/articles/international-perspective-the-electrochemical-mold-polishing-advantage.


Technical Guides

Browse all technical guides →

/* data-no-optimize is REQUIRED: LiteSpeed rewrites plain inline scripts to type="litespeed/javascript", which browsers never execute. This site's existing inline scripts already use the same attribute. */