We help buyers clear the texture question before a tool is quoted, not after the first grained trial. Draft on a grained wall follows the grain depth, not the drawing: Standex Engraving Mold-Tech now asks for 1° per 12.5–15 µm of texture, and two to three times that figure wherever the plastic shrinks onto steel.

There is still no single number for draft on a textured wall. A colour chip fixes the grain, the print carries a one-line note about it, and the quotation is issued long before anyone checks whether the two agree.

One camp copies the angle from the previous program. The toolmaker adds a degree where the walls look steep, the part drops out at trial, and the figure is never revisited. The other camp treats draft as a constraint settled before steel is cut, because a grained wall grips through thousands of microscopic undercuts, and the scuff a dragging part leaves cannot be polished back afterwards.

Speak to the texture suppliers and the fault line becomes visible. Standex Engraving Mold-Tech states plainly that the older recommendation — 1.5° of draft per 0.001 in. of texture depth, roughly 25 µm — no longer holds, and replaces it with 1° per 0.0005 to 0.0006 in., or 12.5 to 15 µm. The old figure still sits on most drawings. Applied to the same 50 µm grain, the two rules sit 0.3° to 1° apart, and on a wall that shrinks onto the core the gap widens to 2° or more.

Four questions frame what follows:

  • What actually sets the draft angle on a grained wall, and where does the requirement come from?
  • How much draft does each texture depth need, and how far apart are the published rules?
  • Which walls force the figure to double, and what decides that call?
  • What must the steel look like before it is textured, and what has to be corrected first?

Short answer, assembled from four published rules and the shop facts we publish ourselves. Draft on a textured wall is fixed by two things: the grain depth, and the direction the plastic moves as it cools. Standex Engraving Mold-Tech asks for 1° per 12.5 to 15 µm on a wall the part shrinks away from, and 2 to 3 times that where the part grips steel. The SABIC processing guide lifts the floor for reinforced compounds to 1° per side against 0.5° for unfilled grades, then adds 1° per side for every 0.001 in. of texture. Run those rules across a 50 µm grain and the published answers spread from 3.0° to 5.0°. The steel also has to reach the engraver free of EDM scale, which is a toolroom decision taken weeks before the first grained trial.

Key takeaways

  • Grain depth sets the floor: Standex Engraving Mold-Tech asks for 1° of draft per 12.5–15 µm of texture on a wall the part shrinks away from, against the older 1.5° per 25 µm figure.
  • Direction doubles the figure: a wall the part shrinks onto needs 2 to 3 times the shrink-away value, so one grain can call for 3.3–4° on one face and 6.6–12° on the face beside it.
  • The rules spread by 2°: at a 50 µm grain the four rules compared here run from 3.0° under the legacy figure to 5.0° for a sharp pattern, a window that decides pass or fail at trial.
  • Reinforced grades start higher: the SABIC processing guide sets a 1° per side minimum for reinforced compounds and 0.5° per side for unfilled grades, then adds 1° per side per 0.001 in. of texture depth.
  • Steel finish comes first: texture below 20 µm needs a 500 emery finish, 20 to 100 µm needs 400 emery and above 100 µm needs 320 emery, with EDM scale removed before etching.

Methodology

How this piece was put together. Every draft figure quoted here comes from a published document, and none of it is a measurement taken in our own works. The rules are drawn from four sources: the Standex Engraving Mold-Tech technical data sheet for textured surfaces, a PlasticsToday article on texturing faults written by a member of the Mold-Tech technical team, the SABIC injection molding processing guide covering LNP compounds, and the SPI mould finish grades, the twelve-level scale the trade uses to name polish from A-1 to D-3. Where a table turns a published rate into a draft angle at a given depth, that arithmetic is ours and is marked as derived. The shop details reproduced below match what we publish on the capability pages. No texture trial was run for this article.

What actually sets the draft angle on a grained wall?

A grained wall releases against more than friction. Chemical etching cuts a pattern of microscopic pits into the mould surface, and molten plastic fills every one of them. On ejection the part must shear out of that interlock across the whole grained area at once. A polished wall only has to slide.

The requirement therefore has two parts. The first is a base draft that comes from the material and the direction of shrink. The SABIC processing guide puts ordinary walls at 2° to 3° per side wherever the geometry allows, with a floor of 0.5° per side on unfilled compounds. Reinforced grades get a higher floor, 1° per side, and the guide gives the reason directly: reinforced compounds shrink less than neat resins. A glass-filled part holds its size, so it stays in contact with the steel for longer and needs a wider angle to leave.

The second part is the texture add-on, and it stacks on top of the base rather than replacing it. SABIC states it as 1° per side for every 0.001 in. of texture depth. Standex Engraving Mold-Tech is firmer still, and its own data sheet is the document that retired the 1.5° rule. Neither figure is negotiable at the trial stage, because draft lives in the steel, and correcting it means polishing the grain back and cutting again.

How much draft does each texture depth need?

The four rules compared here disagree, and the disagreement grows with depth. Each column below applies one published rate across four grain depths, so the numbers are derived from the rule rather than measured on a tool.

Texture depthLegacy rule (1.5° per 25 µm)Standex current (1° per 12.5–15 µm)Rounded pattern (2° per 25 µm)Sharp pattern (2.5° per 25 µm)
12.5 µm (0.0005 in.)0.75°1.0°1.0°1.2°
25 µm (0.001 in.)1.5°1.7–2.0°2.0°2.5°
50 µm (0.002 in.)3.0°3.3–4.0°4.0°5.0°
100 µm (0.004 in.)6.0°6.7–8.0°8.0°10.0°

Read down a column, not across a row. The same 50 µm grain draws 3.0° under the old rule and 5.0° for a sharp pattern.

Two observations sit behind the table. The supplier that published the legacy rule is the one that retired it, which is why the middle column runs above the first. And a sharp-edged pattern needs more angle than a rounded one at the same depth, because the pits cut deeper into the surface for a given nominal figure. But this does not settle the whole picture, since pattern orientation and wall height still change the force a part has to overcome.

Two mirrored black housings moulded as a family cavity set, each half releasing against a different shrink direction
Two halves of one family tool, each releasing against its own shrink direction

Where does the draft have to double?

Shrink direction decides more than grain depth does, and it is the input buyers leave off the drawing most often. A cavity wall lets the cooling part pull away from the steel. A core wall does the opposite: the part contracts onto the steel and grips it. Standex Engraving Mold-Tech resolves the difference in one line of its data sheet, asking for 2 to 3 times the shrink-away figure on anything that shrinks onto the tool.

Feature or conditionDraft requirementSource
Wall the part shrinks away from (cavity side)1° per 12.5–15 µm of texture depthStandex Engraving Mold-Tech data sheet
Wall the part shrinks onto (core side, internal features)2 to 3 times the shrink-away figureStandex Engraving Mold-Tech data sheet
Sliding cores, lifters and angled facesSet from the component angle of action, not the draw directionStandex Engraving Mold-Tech data sheet
Shut-off along a grained sidewallAdditional draft, or special preparation before releaseStandex Engraving Mold-Tech data sheet
Unfilled compound, smooth wall0.5° per side minimumSABIC injection molding processing guide
Reinforced compound, smooth wall1° per side minimumSABIC injection molding processing guide
Any grained wallAdd 1° per side per 0.001 in. of texture depthSABIC injection molding processing guide

The direction of shrink doubles the figure. A mirrored core can need twice the draft of the wall beside it.

Slides and lifters bend the rule further, because they move along their own axis rather than the draw direction. A textured face on a lifter is judged from the angle it travels, and the same face on the fixed half would be judged from the draw. Where a grained wall also serves as a shut-off, the two surfaces need to seal against melt while still releasing a textured part, which is why that combination attracts extra draft or bench work. Glass-filled and recycled feeds sharpen the same problem, and the wear they leave on the tool is covered in a separate note on steel selection for filled and recycled resins.

What finish must the steel carry before it is textured?

Draft is only one half of the preparation. The surface the engraver receives decides whether the pattern transfers cleanly, and the requirement scales with the depth being cut. A finish that is too coarse shows through the grain. Leftover EDM scale is worse: it etches unevenly and cannot be recovered after the fact.

Texture depth to be appliedEmery finish required firstRelated requirement
Below 20 µm500 emeryEDM scale fully removed before etching
20 to 100 µm400 emeryCutter marks and burn marks removed
Above 100 µm320 emeryWeld repairs confirmed before texturing

Finish the steel before the engraver sees it. EDM scale left in place etches unevenly and stays hidden under the pattern.

The data sheet names the tool steels that texture reliably: P-20, H-13, S-7, O1, A1, A2, A6, 420 stainless, beryllium copper, kirksite and both forged and cast aluminium. It also sets out a short list of checks that belong to the toolroom rather than the engraver, including steel quality and inclusions, the standard of any weld repair, and a 220 aluminium oxide pass that reveals areas likely to scuff. Scribe lines on a flat shut-off go on with a laser, because a hand-cut line is another surface the melt can catch. In our shop the cavity work, the spark eroder and the surface grinder sit in the same building, so the finish a grained insert leaves on is a decision we make rather than a handover.

Multi-cavity mould plate with cooling ports and inserts checked before the plate returns to the press
A multi-cavity plate checked insert by insert before the trial

Limitations

None of the draft angles in this article were measured on a mould in our shop. They are published rules, applied to a depth to show the arithmetic behind them. A real part adds texture orientation, wall height, ejection layout and mould temperature, and no single number carries all four. Treat every angle here as a starting point that a trial has to confirm.

The four rules come from four documents, and they do not agree with one another. Standex Engraving Mold-Tech writes for the texturing trade, the SABIC guide writes for moulders of reinforced compounds, and the SPI and VDI 3400 scales describe surface classes rather than draft. Where the documents conflict, this page shows the range instead of choosing a winner. The resin data sheet for a specific grade, not this article, decides how much that grade shrinks.

Documents consulted for the draft rules: the Standex Engraving Mold-Tech technical data sheet, cdn.mold-tech.com/wp-content/uploads/2020/01/SMT-Technical-Data-Sheet.pdf; PlasticsToday, Mold Texturing Pitfalls and Solutions, plasticstoday.com/injection-molding/mold-texturing-pitfalls-and-solutions; the SABIC injection molding processing guide for LNP compounds, sabic.com/en/products/documents/lnp-konduit-compounds-portfolio-introduction/en; and the SPI mould finish grade scale alongside VDI 3400.

What this means for your RFQ

We help buyers settle the texture question while the tool is still a drawing. Two inputs decide the draft, and both belong in the enquiry: the grain grade or depth, and a note on which faces the part grips as it cools. Send a STEP file with the texture callout and the resin, and the draft can be reviewed against the grain before any steel is cut. Leaving the texture depth or the shrink direction out is what restarts a program later, the same pattern that three missing RFQ inputs leave on the schedule. From a small grained cover to a deep-ribbed housing, the draft is cut once and checked at first article.

Send the drawing and the texture note to info@hongqiangmould.com. A quotation comes back within 24 hours. Drafted | Grained | Measured

Frequently asked questions

How much draft does a textured mould need? The figure depends on the supplier. Standex Engraving Mold-Tech recommends 1 degree of draft per 12.5 to 15 micrometres of texture on a wall the part shrinks away from, and two to three times that figure where the part shrinks onto steel. The older rule of 1.5 degrees per 25 micrometres is no longer recommended.

Why do reinforced plastics need more draft than unfilled grades? The SABIC processing guide sets a minimum of 1 degree per side for reinforced compounds and 0.5 degree per side for unfilled grades. Those grades shrink less than neat resin, so the part stays in contact with the steel longer and the guide raises its floor. The same guide adds 1 degree per side for every 0.001 inch of texture.

Does a deeper texture always need more draft? Yes, within a single rule. Every published rule compared here scales the draft with texture depth, so a 100 micrometre grain needs more angle than a 25 micrometre grain. The rules differ in how fast the figure climbs. A sharp-edged pattern also needs more than a rounded one at the same depth.

Can the draft be corrected after the mould is textured? It can, but at a higher cost. A grained surface has to be polished back before the angle can be recut, then grained again, and the second etch rarely matches the first. Settling the draft before texturing is cheaper than changing it afterwards. Send the grain depth with the drawing so both are fixed together.

What steel finish is needed before texturing? Standex Engraving Mold-Tech asks for a 500 emery finish on areas textured below 20 micrometres, 400 emery between 20 and 100 micrometres, and 320 emery above 100 micrometres. The surface must be free of EDM scale, cutter marks and burn marks first. That preparation belongs in the toolroom, before the engraver receives the insert.

Jack works on the tooling and molding team at Hongqiang Mould, an injection mould manufacturer and plastic injection molding supplier. The shop runs 11 presses from 80 to 450 T, 5 CNC machining centres and a metrology room with bridge CMM inspection.


Technical Guides

Browse all technical guides →